TECHNET Archives

March 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "lduso - Diamond-MT.com" <[log in to unmask]>
Date:
Mon, 20 Mar 2017 12:50:55 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steven Creswick <[log in to unmask]>
Message-ID:
Subject:
From:
Steven Creswick <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (123 lines)
Bob,

I've used SCS in Indianapolis, but they have many other branches.

Is a batch process.  Cost is in masking, if required.  Typically, the labor
intensive part.

Call them and find out

Steve

https://scscoatings.com/
​

On Mon, Mar 20, 2017 at 12:46 PM, lduso - Diamond-MT.com <
[log in to unmask]> wrote:

> Bob
>
> Considering parylene is all done by batch process, pricing has a much to do
> with that batch size, The largest effect on cost is the prep time. Masking
> is labor time and that is costly. Parylene materials are pricey but not
> outrageous. Let me know if you want more details.
>
> Lloyd Duso
> Plant Manager
> Diamond-MT
> (814) 535-3505
> www.Diamond-mt.com
>
> On Mon, Mar 20, 2017 at 12:05 PM, Robert Kondner <
> [log in to unmask]>
> wrote:
>
> > Torsten,
> >
> >  Do you know how thick a parylene coating is? My recollection is pretty
> > thin.
> >
> >  So I checked, very high dielectric strength, thickness typically under 1
> > mil but it can be built up further with longer processing time.
> >
> > Any idea wat coating with parylene cost for a small batch of boards?
> >
> > Thanks,
> > Bob Kondner
> >
> >
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of Torsten Hagge
> > Sent: Monday, March 20, 2017 9:17 AM
> > To: [log in to unmask]
> > Subject: [TN] WG: [TN] Screen On Insulation
> >
> > Hi,
> >
> > cheap solution could be a 1mil kapton tape with the mention risk of air
> > gaps, fine and cost expensive solution parylene HT  coating before
> placing
> > the ferrite cores...
> >
> > Take care
> > Torsten
> >
> >
> >
> > Best Regards
> >
> > KRISTRONICS GmbH
> >
> > Dipl.Ing. (FH) Torsten Hagge
> > team leader HW development
> > Gewerbegrund 5-9
> > 24955 Harrislee
> > Telefon +49 (0) 461 7741-624
> > Telefax +49 (0) 461 7741-642
> > [log in to unmask]
> > www.kristronics.de
> > Place of jurisdiction: Flensburg, commercial register: HRB 1433 FL
> > CEO Dipl.-Ing. oec. Thormod Ohm
> > VAD-Id DE 811182059
> > Bank account: Deutsche Bank AG Flensburg, account 4216610, bank number
> > 21570011
> > IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215
> >  Please consider the environment before printing this e-mail
> >
> >
> >
> > -----Ursprüngliche Nachricht-----
> > Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Robert Kondner
> > Gesendet: Freitag, 17. März 2017 21:11
> > An: [log in to unmask]
> > Betreff: [TN] Screen On Insulation
> >
> > Hi,
> >
> >
> >
> > We have a PCB that turns out to require 2500VAC test for 60 seconds and
> we
> > had some flash over on pads to vias. We also have a planar ferrite
> > transformer with primary windings on one side.
> >
> >
> >
> > Does anyone know of a screen on insulation material that can be used to
> > increase flash over voltages? I would like to get a 2 or 3 mils of
> material.
> > My other option is to have a laser cut layer of isolation but that could
> > leave air paths under the material.
> >
> >
> >
> > Any other ideas welcome.
> >
> >
> >
> > Thanks,
> >
> > Bob K.
> >
>