TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, James TerVeen <[log in to unmask]>
Date:
Wed, 2 Nov 2005 20:28:45 -0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Greig <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
David Greig <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)
Oops, should have said /98.

Slash sheets are better than nothing, but I always find them playing the lowest denometer and not going far enough to be a tight
description of all the material parameters that we are usually face with.
For example, Dk and Df over say 1MHz to 1GHz(or 10GHz) and at a specific resin content.
Volume and surface resistivites that are closer to real materials would be really useful for sensitive analog designs.


Best Regards

David Greig
______________________________
GigaDyne Ltd
http://www.gigadyne.co.uk
______________________________

-----Original Message-----
From: David Greig [mailto:[log in to unmask]]
Sent: 02 November 2005 19:29
To: 'TechNet E-Mail Forum'; 'James TerVeen'
Subject: RE: [TN] board material for high temp

4101A/96 would be a good starting point, until 4101B comes out. Look for phenolic resin or non-dicy systems.
All the majors have newish materials. Td >= 300 is a useful metric, and I assume that all 4101B sheets will have this and Tg as
well (what about having relative moisture absorption rates?).

Best Regards

David Greig
______________________________
GigaDyne Ltd
http://www.gigadyne.co.uk
______________________________

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of James TerVeen
Sent: 02 November 2005 19:14
To: [log in to unmask]
Subject: [TN] board material for high temp

What does everyone us for board material for High temperature solder
applications.   We have a new product that will require the use of high
temperature solder.   Will the use of conventional FR4 be sufficient.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC
web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at
[log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
--
Virus scanned by Lumison.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2