TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Dehoyos, Ramon
Date:
Mon, 28 Nov 2005 09:49:38 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (66 lines)
        1 micron = 1/1000000 of a Meter
        1 micron =   1/1000 of a mm
        1 mil =      1/1000 of in
        1 micro in = 1/1000 of a mill
        1 micro in = 1/1000000 of in
        1 mm = 1/25.4 in = 0.0393 in = 39.3 mils
	
                                   1 mm      1 in                 1000000 microns	
        1 micron          X     ---------        X      ------     X   --------------  =  39.3 micro in
                              1000 microns      25.4 mm            in






-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez
Sent: Monday, November 28, 2005 9:24 AM
To: [log in to unmask]
Subject: Re: [TN] Intermetallic Layer

I have been stating all along that MICRONS are a SMALLER unit of measure than MICRO INCHES.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Indrek Rebane
Sent: Monday, November 28, 2005 7:56 AM
To: [log in to unmask]
Subject: Re: [TN] Intermetallic Layer

Hi Victor,

Victor G. Hernandez wrote:
> Microns are smaller units of measure than MICRO INCHES.

You seem to be confusing microinches with mils. One microinch is thousandth of mil, which is thousandth of inch. One microinch is 0.0254 microns.

Indrek,
Actually a proponent of the SI (Metric) system.

--
Indrek Rebane
Borthwick-Pignon OÜ, R&D
Riia 185, 51014 Tartu, Estonia
Phone: +372 7 302 641, Fax: +372 7 383 041

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2