TECHNET Archives

January 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="windows-1252"
Sender:
Subject:
From:
Dave Chapman <[log in to unmask]>
Date:
Thu, 16 Jan 2003 14:11:32 -0600
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Carlr Ray <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Dave Chapman <[log in to unmask]>
Parts/Attachments:
text/plain (61 lines)
1:1 only on alternate finish like Immersion Silver and Gold where you don't
have a solder base already. Otherwise we reduce everything 10%. Make all R's
and C'(even alternate board finishes) home plate design....bingo no more mid
chip beads (solder balls)
Dave C.
Manufacturing Engineer
Circuit Service Inc.

-----Original Message-----
From: Carlr Ray [mailto:[log in to unmask]]
Sent: Thursday, January 16, 2003 1:41 PM
To: [log in to unmask]
Subject: [TN] Stencil Aperture Mod


How many of you guys still run product with 1:1 apertures? How many
commonly use reduced or modified apertures?

I have an issue where I can not convince some other Engineers that
modifying the apertures to correct for solder balling is a good
solution.

The process is a no clean process and the profile meets the solder
paste manufactures recommended parameters.

The solder ball appear on next to the middle of the parts (like solder
escapement) and some are trapped by the flux others or not.

Do you guys know of any standards that address these issues?

Carl Ray
Sr. Manufacturing Engineer
Huntsville, AL 35807
Phone: 256-882-4800 ext. 8845
Cell: 256-990-1990

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2