Dan, you didn't mention if you bake before use. I suggest you have a
sample of each batch baked for at
2-4 hours at 220(F just before wave solder and re-test. You may have a
moisture problem.
----------
From: [log in to unmask][SMTP:[log in to unmask]]
Sent: Monday, December 09, 1996 7:41 AM
To: [log in to unmask]
Subject: Soldermask peeling
We recently experienced soldermask peeling after wave from
three different Fabricators all within 2 weeks. Subsequently
we took sample lots of each Fabricator and performed a
pre-wave and post-wave tape test. In all lots the boards
passed pre-wave tape test but had a 10-25% failure post wave.
What can cause this phenomena? Does the weather change have
anything to do with soldermask application and durability?
Dan Hickey
Senior Buyer
Vicor
[log in to unmask]
**************************************************************************
*
* TechNet mail list is provided as a service by IPC using SmartList v3.05
*
**************************************************************************
*
* To unsubscribe from this list at any time, send a message to:
*
* [log in to unmask] with <subject: unsubscribe> and no text.
*
**************************************************************************
*
* If you are having a problem with the IPC TechNet forum please contact
*
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]
*
**************************************************************************
*
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|