Scott, here at Circo Craft we have been using conveyorized inner layer oxide
and reduction processing for over 8 years. It works very well and uses
standard, commercially available oxide and reduction chemistries.
Dave Rooke
Circo Craft - Pointe Claire
___________________ reply separator ___________________
>I am currently in the design phase of a new 45,000 sq. ft. pcb
>manufacturing plant and I'm wondering if I should build a new BLACK OXIDE
>line with all the associated baskets and handling labor - or consider a
>conveyorized process such as DuraBond or ???.
>
>Can anyone give me some information on their opinions about a
>conveyorized method of chemical preparation prior to Lamination?
>
>
>Scott McCurdy, president
>McCurdy Circuits
>Orange, California
>
>(714) 974-0401
>[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|