Hi Doug,
The only no-clean ROSE testing we do is for qualifying a new solder paste or other no-clean chemistry. The test would be on non production boards so they would be
scrapped.
Experience the benefits of Precision Engagement
Brien Bush
Manufacturing Applications Specialist
Phone: 603.249.9190 | Fax: 603.249.9192
[log in to unmask] www.cirtronics.com
ISO 9001 & 13485 Certified
Follow us on LinkedIn|Friend us on Facebook
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Friday, December 04, 2015 11:57 AM
To: [log in to unmask]
Subject: [TN] ROSE on No-Clean Assemblies
Good morning all,
As you wrestle with Dave's element question, I have a question or questions for you.
For those of you who are manufacturing product using no-clean technology and no cleaning, Do you do ROSE testing on the no-clean units and if so, do you consider the ROSE tested assembly still viable or is it scrapped?
If you want to reply off-channel, that is fine. Thanks.
Doug Pauls
Principal Materials and Process Engineer Rockwell Collins
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
WARNING: Export Control This message, including any attachments, may contain technical data within the definition of the International Traffic in Arms Regulations (ITAR), and subject to the Export Control Laws of the U.S. Government. Transfer of such information by any means to a foreign person, whether in the United States or abroad, without proper export authorization or other approval from the U.S. Department of State is prohibited.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|