TECHNET Archives

June 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Cash, Alan" <[log in to unmask]>
Date:
Tue, 15 Jun 1999 12:40:24 -0700
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum.\" <[log in to unmask]>, \"Cash, Alan" <[log in to unmask]>
Parts/Attachments:
text/plain (76 lines)
The solder plating has no barrier layer? I assume that it is not fused
either.  Then the copper from the bronze has migrated to the surface of the
porous solder plating and has oxidized.  It is doubtful that you can wave
solder the terminals in this condition with no-clean flux.  The terminal may
require stripping.  Did you question the manufacturer about the difficulty
in soldering?  They may have some suggestions.

Al Cash

        ----------
        From:  Kathy Stillings [SMTP:[log in to unmask]]
        Sent:  Tuesday, June 15, 1999 10:49 AM
        To:  [log in to unmask]
        Subject:  [TN] Lead solderability

        Hi technetters,
        Hope all is well.....................  Got a quick question - I am
using Power
        chip resistors (manufacturers name with held :) ) that have a
"solder plated
        phosphor bronze" terminal.  I am having a bugger of a time soldering
these
        parts.  I have limited solderability testing capabilites and am
forced to use
        the old solder pot test to verify solderability.  I get good solder
adhesion on
        some and very poor on others.  I don't have any experience with
phosphor bronze
        based terminals.  I am looking for your expertise on how I can wave
these parts.
        Note:  leads are very dark in color as if they are contaminated but
the date
        codes on the parts is very new. Oh yeah - sodler is 63/37 with no
clean alcohol
        base flux spray.

        Thanks again in advance for the help!

        ################################################################
        TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
        ################################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
        To subscribe:   SUBSCRIBE TechNet <your full name>
        To unsubscribe:   SIGNOFF TechNet
        ################################################################
        Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
        For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
        ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2