TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Date:
Fri, 15 May 2009 08:22:28 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
John Foster <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
A<002a01c9d55f$795eb8b0$6c1c2a10$@com>
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
There are no holes, its merely an etch and coverlay. Its simple traces going from one end to the other. I will speak with the fabricator about the direction.

Thanks





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Kelly

Sent: Friday, May 15, 2009 6:17 AM

To: [log in to unmask]

Subject: Re: [TN] FLEX question



Hi John,

If the part was built as a pattern plate versus a button or selective plate it will most likely fail. If copper is plated on the top of the tracks you now have approx. .0014 of RA copper with probably about .0007 - .001 of plated copper on top AP 9121 should be specified as AP 9121R for rolled annealed. Good luck. Steve Kelly



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of John Foster

Sent: May-14-09 10:08 PM

To: [log in to unmask]

Subject: Re: [TN] FLEX question



Hi Werner

1. When I looked up pyralux AP-9121 it said it was a 2 mil core 1/1. 

2. This should be the normal bend radius. I have to look into the mechanical situation 

    More tomorrow. That’s one reason I am concerned about the number of installs and deinstalls. I have had people fold flexs in half and then wonder why they break.

3. The fracture seems to be about halfway down the middle of the flexed leg.

4. That’s why I brought up the 17 mil traces they have not fractured.

5. When I saw the datasheet from Dupont it said the material came in both electro depostited and rolled annealed copper. However I typed in AP-9121 on the internet and

The dupont pyralux material came up which claims to be annealed. However all the fabricator told me is that they used AP-9121 is this like calling out FR-4 in the rigid world. Is Ap-9121 a Dupont name or could the material have come from many different laminate suppliers?

Thanks







-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*

Sent: Thursday, May 14, 2009 6:29 PM

To: [log in to unmask]

Subject: Re: [TN] FLEX question





 Hi John,

Unfortunately, you do not give us an adequate picture of the situation.

Missing:

1) 2-mil core thickness, the critical dimension is 1/2 of core plus 2x1.4 mils=2.4 mils [not exactly small];

2) bend radius, approximately .35 inches could be an average with minimum much smaller depending on who and how the bend is made;

3) fracture location is not clear, open is about in the middle of the flexible section—does that mean half-way between the stiffener and the connector?

4) any cracks in the 17-mil wide traces?

5) While you say the CU is rolled annealed, have you confirmed the anealing—if not annealed the ductility in the rolling direction will be significantly larger than X-rolling direction—you can tell be etched x-sections showing needle-like grains in the rolling direction;

Obvious:

1) Crack propagation being roughly equal, the 8-mil trace will show an open first;

2) if not fully annealed, rolled Cu direction should be along flexed leg.



Werner





 





 



-----Original Message-----

From: John Foster <[log in to unmask]>

To: [log in to unmask]

Sent: Thu, 14 May 2009 8:52 pm

Subject: [TN] FLEX question





















I was hoping I could get some input on a problem we are having with a

flex circuit.



 



I have a 2 layer flex circuit that is shaped like a L. one leg is about

5 inches long the other leg is about 4 inches long



At the corner of the L is a stiffener on both sides. The stiffener

extends into both L sections a very small amount about=2

0.3 inches.



Both ends of the flex have Omnetics connectors which are designed to be

soldered onto flex circuits. The A28300 series. Some of the traces are

17 mils wide and some are 8 mils wide. The traces are spaced fairly

evenly across the flex and are spaced like the omnetics connector which

means you can't see through the circuit as the traces overlap from side

to side.  One section of the L flexs the other section is stationary.

The bend radius for the flexible section is approximately .35 inches ( I

am not positive of this number and will find out tomorrow but I know it

is far more the 6X of the thickness). The flex is constructed as follows



 



The core is   AP-9121 with 1 oz copper on both sides.



The coverlays are LF-0110



The adhesive for the stiffener is LF-0200



And the stiffeners are .028 FR-4



The edges of the stiffeners are beaded with  emerson & cummings ecobond.



I have spoken with the fabricator and they assure me that the copper is

roll annealed and not electro deposited.



The flex circuit has failed after less than 1000 cycles. The cycles are

very slow and maybe 10 or 20 per day. 



The current going through the traces is very low on the order of 10 mA.



 



We have had two circuits fail and they both have failed on the 8 mil

traces. I have scraped the coverlay off of the flex and have concluded

that the open is about in the middle of the flexible section but I can't

see it. I would have expected to see an open at the=2

0end of the coverlay

as I have seen this before. We have been potting the connectors to move

the stress point from the omnetics connector pins to further down the

flex past the end of the coverlay. 



  I have a couple of questions.



1.       Is there a way to remove the coverlay without using mechanical

means I fear that I could screw up the sample by scraping it with a

razor.



2.       Does this surprise anyone that it would fail this soon with a

bend radius that I know is large and only a 2 mil core?



The flex has been removed many times from the system and reinstalled and

I am still having a hard time convincing people that flex circuits must

be treated with care. i.e. can't be laid on benches and smashed.



Tomorrow I will get to get into the system and see the mechanicals but

the mechys assure me that at no time is the flex stretched to the point

of pulling the bend radius down. I soldered a wire onto the connector

and ran a needle up and down the scraped flex and it sure seems as

though it opens about in the middle of the flexible section. 



 



Anyway any input will be appreciated 



Thank you



 



 





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Techn

et NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 

additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815

-----------------------------------------------------







 





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2