Dear Technettes
One of our PCB Manufacturers has recently started using the "Omikron"
(Immersion White Tin) process as an alternative to Hot Air Leveling.
They are asking us (the designers) whether they can use it for our boards.
I've looked through the archives, and there seem to be no major problems
noted so far. Still, it's a couple of months since it's been discussed,
and it is a new(ish) process. So, here goes :
Does anyone know of any particular adverse design or assembly implications
of using this process? Do you know (even as hearsay) of any problems with
the process?
Thanks, and Regards
Brian Rusten
Contract PCB Design Engineer
JNA Telecommunications Ltd Ph (02) 9935 5777 Fax (02) 9417 3862
(Now "A Lucent Company")
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|