TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 16 Jun 2005 12:16:52 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Bloomquist, Ken" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Bloomquist, Ken" <[log in to unmask]>
Parts/Attachments:
text/plain (25 lines)
Hi Steve and Ramon,

I'll answer Ramon's question first;
"Is this the first time that you run this board through the wave?"
No, we've run them before and had much better results. We will give
baking them a try.

Steve, they are not pressed in hard at all. They are in hard enough to
keep the perpendicular through the wave process but you can still turn
them with your fingers after they are swaged.

The holes are actually quite large, .191".

KennyB

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2