TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Jana L. Carraway" <[log in to unmask]>
Date:
Mon, 26 Mar 2001 12:41:17 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ted Stern <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Ted Stern <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)
Dear Ms. Carraway:

Regarding your question on cupric etch rate/profile, it has been my experience mechanical
variables (spray pressure, nozzle density, nozzle type, rate of etchant flow, spray/ocillation
pattern, distance from the nozzle to the panel, guide roller interference with spray, etc.),
have a larger inpact on etch rate than acid normality.  We have recently profiled
approximately 30 cupric etchers in an attempt to correlate overall etching performance (speed
and etch factor) based upon mechanical and chemical variables; and it is likely a performance
estimation for your etcher could be made by comparing it with data gathered thus far.  (Please
e-mial or call me at (763-479-6525) if you would like a copy of the profile forwarded as an
e-mial attachement.)

Regards,
Ted Stern

"Jana L. Carraway" wrote:

> Greetings IPC TechNet Forum!
>
> I am in search of information on two topics: 1)Etch rates/factors for cupric
> chloride etchant and 2) current carrying capacity of very fine lines.
>
> 1) With respect to Cupric Chloride etchant, does anyone have information
> they would be willing to share on the etch rate and etch profile?  My dusty
> brain cells seem to remember that the etch rate increases with acid
> normality, but that the lateral etch increases as well.  I have it in mind
> that for fine line, an acid normality of around 1.0 N produced the best etch
> factor, although affected the speed/throughput.  Would anyone have a bit of
> information they could share on this?
>
> 2) My copy of the Printed Circuit Manufacturing book has current carrying
> capacity vs line width down to 0.020" lines.... I am looking for the current
> carrying capacity of 25, 50, and 75 micron lines.  Could someone point me in
> the direction of this information?
>
> I greatly appreciate the help.
> Best Regards,
> Jana Carraway
>
> Jana Carraway
> Micro Systems Engineering, Inc.
> 6024 SW Jean Road
> Lake Oswego, OR  97035
> 503-635-4016
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2