TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Tue, 21 Jun 2005 07:49:30 -0400
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Collins <[log in to unmask]>
Subject:
From:
Graham Collins <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (109 lines)
Hi Steve!
Had a great Father's day - how my 6.5 month old dragged that bottle of
scotch in I do not understand, but I'll take it.  Whoo-hoo!

As for MSL levels, we are seeing some of the same thing I think you
are.  We buy lots of parts through distributors, who repackage them in
the small quantities we need.  The packaging they use sometimes
indicates a MSL level a couple of values higher than it should.  Just a
few days ago our SMT operator had me check one where he had two
packages, one indicating MSL=2, one indicating MSL=3, and when I checked
the Ti web site it showed a MSL=1.  I'm guessing the distributor is
being overcautious and/or marking it up for lead-free processing.  I
agree, it's a pain - as we have to either err on the side of caution and
end up baking parts that don't need to be baked, or we verify each one
against the manufacturer's data.

regards,

Graham Collins
Process Engineer,
L-3 Communications Electronic Systems Inc.
Halifax
(902) 873-2000 ext 6215

>>> [log in to unmask] 06/20/05 12:25PM >>>
Good mornin' all!

I hope all you Dads out there had a wonderful Fathers Day!

As I posted about a week or so ago, we're getting our stockroom
personnel to really focus on component moisture sensitivity levels.

But now I'm starting to get a little confused about how components
are generally classified with their respective MSL ratings.

I've always thought that it had to do with component body size and
thickness,
but now I'm finding out that it doesn't necessarily.

My stockroom clerk showed me an IDT SOJ28 that came in sealed with a
MSL 3
rating that we now have in our dry box because the package was opened.

We have some Cypress SOJ28's and SOJ24's that are on reels that are not
in
original packaging, so I called Cypress and asked what the MSL rating
is
for the
two part numbers and they are a MSL 1. Cypress gave me a link to the
SRAM
Qualification Report that states that.

Now my stockroom clerk brought me some Vishay tantalum caps that have
a MSL 2a rating label on them, and they are TNTC's. This is THE FIRST
time
I
have ever seen a MSL label on a tantalum capacitor.

Are these ratings based on qualification reports? Or can one look at
the
size and
thickness of the part to base how you will handle it?

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and
confidential to
LaBarge, Inc.  It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or
deliver
this message to anyone.  In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2