TECHNET Archives

February 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Brian Ellis <[log in to unmask]>
Date:
Thu, 28 Feb 2002 20:51:55 +0200
MIME-version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Gaby Bogdan <[log in to unmask]>
Subject:
From:
Gaby Bogdan <[log in to unmask]>
Content-Transfer-Encoding:
7BIT
Content-Type:
text/plain; charset=iso-8859-1
Parts/Attachments:
text/plain (72 lines)
Brian,
I was following with great interest the subject. Right now, I am in the
middle of trying tosolder CSP's with "Flux underfill", and I see
similarities in the problems that could arise. Could you give me some hints
for the reliability of the process?
Gaby
----- Original Message -----
From: "Brian Ellis" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, February 28, 2002 9:10 AM
Subject: Re: [TN] No No-clean?


> OK, there are three issues at stake here.
>
> 1) The residues from "no-clean" products (and yes, there are residues -
> always) may impede adhesion of the coating layer to the substrate
>
> 2) Many of the "no-clean" products rely on a slow sublimation of the
> residues from the surface, requiring a few weeks to achieve optimal
> performance. Sealing these in will prevent this from happening.
>
> 3) By definition, all soldering fluxes are ionic. Some may be slightly
> hygroscopic, as may also the metal salts formed by the reaction between
> the oxides and the flux acids. Some of the rheological additives to
> pastes may leave slightly hygroscopic residues. This is an open
> invitation to promote vesication, with a potentially very serious loss
> of reliability. At the very least, a good "pressure cooker" test is a
> must both in qualifying the process and at frequent intervals to check
> that it stays on the rails.
>
> I am not saying that coating should never be applied over flux residues.
> What I am saying is that anyone who does it without a really thorough
> qualification and process control is being professionally irresponsible,
> if the products must be reliable. After all, conformal coating is really
> a high-rel process and "no-clean" chemistry started as a low-rel
> process, creeping up to its present status of medium-rel. It is
> therefore really a paradoxal conflict to try and combine the two, likely
> to present the disadvantages of both processes with none, or few, of the
> advantages.
>
> Brian
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2