Joel,
Section 6.8 of IPC-A-610C covers HV soldering. I can tell you from several
years experience with HV soldering that the illustrations must be used as
guidelines only. It is near impossible for an operator to make a perfect
sphere or hour-glass shape as shown in the illustrations. Inspectors must be
aware of this. The important point to remember is that all joints must be
smooth, that is, no sharp edges or protrusions. Also see paragraph 13.2.3 of
J-STD-001C.
Bob
Robert Barr
Manufacturing Engineering
Formation, Inc.
Voice: 856-234-5020 x3035
Fax: 856-234-6679
email: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Joel Miller
Sent: Wednesday, October 25, 2000 8:25 AM
To: [log in to unmask]
Subject: [TN] Ball soldering for high voltage PCB assembly
I am new to this list.
I am looking for information pertaining to Ball Soldering for high voltage
PCB assembly.
Is there a IPC standard or a procedure on how to do this technique?
Joel Miller
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|