i have to ask.  are we talking enig or electoplated nickel and electroplated gold?

-----Original Message-----
From: Eric CHRISTISON [mailto:[log in to unmask]]
Sent: Tuesday, May 04, 2004 6:18 AM
To: [log in to unmask]
Subject: [TN] Corrosion resistance of Ni/Au plating


Folks,

We've just carried out some qualification tests on a socket which was reflow
soldered to a board whose pads were plated with Ni/Au. As far as I know a
'standard' Sn/Pb solder was used.

The results of the salt spray test were not a pretty sight. The solder
joints corroded to a point where, in some cases, the socket fell off the
board.

Is Ni/Au a particularly bad finish for corrosion resistance and, if so, what
would be the best?

Alternatively is Ni/Au generally good but are there any defects in the
plating/pcb that can cause a failure in such a test?

Also, does anyone know if the corrosion resistance of lead free alloys are
better or worse than the Sn/Pb we all know and love?

Thanks,


Eric Christison Msc
Mechanical Engineer
Consumer & Micro Group - Imaging Division
STMicroelectronics
33 Pinkhill
Edinburgh
EH12 7BF
UK

Tel:     +44 (0) 131 336 6165
Fax:    +44 (0) 131 336 6001

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2