TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 18 Jul 2005 14:00:13 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (101 lines)
Hi Steve! The IPC-7095A document is a guidelines document and does not
contain specific acceptance/rejection requirements. Paragraph 7.5.1.7 lists
the JSTD-001/IPC-610 specifications as containing the acceptance/rejection
criteria. Those drawing notes should only be referencing the
JSTD-001/IPC-610 specifications.

Dave Hillman
Rockwell Collins
[log in to unmask]




             Stephen Gregory
             <Stephen.Gregory@
             LABARGE.COM>                                               To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             07/18/2005 01:07          [TN] BGA voids
             PM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
             Stephen.Gregory@L
                ABARGE.COM






Good Day Technetters!

I have a question about BGA voids. We are bidding on some
work and it looks like they have taken statements that are in the IPC-7095,
and placed them as notes on their drawing.

One of the notes has to do with a limit on the percentage of balls on a BGA
device that are allowed to have voids. For example; "Less than 5% of the
balls can have voids, and the percentage of the void area must meet class
3 requirements."

I can understand the void area being critical, but the percentage of the
number of balls that are allowed to exhibit them?

The reason that I'm asking, is that I was told last week by a application
engineer from a x-ray machine company (who shall remain nameless),
that seeing voids is normal. Just as long as they aren't too big, or being
concentrated at either the pad/ball interface, or the ball/device
interface.
He said you should worry if you don't see any voids on BGA's with eutectic
balls.

Just curious as to what you all think about this?

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2