I am getting differing information from different suppliers of PWB's with
regard to solder thickness requirements after HASL. Some say 100 to 500
u-inches, others say 500-800 u-inches and yet others say 1200-3000 u-inches
(.0012" to .003"). We are looking for 6 months to one year of solderability
with storage being in an air-conditioned environment with well less than
saturation humidity in the stockroom. (Generally temp is in the 70 to 75
deg F range, relative humidity 50 percentish +/- 10 percentage points.)
Can some one tell me what the height of the "normal" intermetallics is on a
HASLed SMT pad and how much additional solder coating is needed to prevent
deterioration of the solderability of the pads?
Thanks all,
Charlie B.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|