TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=US-ASCII
Sender:
Subject:
From:
Chris Ball <[log in to unmask]>
Date:
Tue, 21 Mar 2006 13:42:48 -0500
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (134 lines)
...we routinely punched dip and sip patterns of 40mil holes on 100mil
centers on 60 mil thick CEM-1. 1x board thickness was considered min
spacing between punched features but we could cheat it a little if we had
to. Maybe because we had 2-stage punch?




                       George Patrick
                       <[log in to unmask]        To:   [log in to unmask]
                       EK.COM>                           cc:
                       Sent by: TechNet                  Subject:    Re: [TN] Die Punching PWBs as opposed to drilling
                       <[log in to unmask]>                   and NC routing

                       03/21/2006 01:14 PM
                       Please respond to TechNet
                       E-Mail Forum; Please
                       respond to
                       george.h.patrick







If I remember correctly...

I don't think we punched anything less than 40 mil [1 mm].  I don't
think there WAS a maximum, but I can't remember punching larger than a
60 mil [1.5 mm] round hole.  We commonly punched slots for relay frame
leads and such that had the long dimension larger than that, though.
Minimum spacing was 1.5X board thickness, but usually that was not a
problem as we used around a 20 mil [0,5 mm] annular ring on the pads and
between minimum spacing and annular ring were usually further apart than
we needed.

The insertion folks preferred the punched boards, too.  The holes were
slightly larger on the insertion side of the board than on the copper
side so they could run the VCD inserters faster than they could for an
equivalent drilled hole (or so they claimed, anyway).

--
George Patrick
Tektronix, Inc.
Central Engineering, Engineering Design Services
P.O. Box 500, M/S 39-512
Beaverton, OR 97077-0001
* 503-627-5272 (voice)     * 503-627-5587 (fax)
http://www.tektronix.com    http://www.pcb-designer.com

"Off-Grid and Proud of it!"


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Monday, March 20, 2006 16:48
To: [log in to unmask]
Subject: Re: [TN] Die Punching PWBs as opposed to drilling and NC
routing


In a message dated 3/20/2006 4:16:28 P.M. Pacific Standard Time,
[log in to unmask] writes:

I would  love to see some cross-section pictures of the plating of a
punched  hole  near the _end_ of a production run :)


I would like to also, George...

If you can recall and don't mind sharing the info, what was he minimum
hole
size you punched and what was the maximum number? Also what minimum
spacing
was  allowed?

Thanks.

Kind regards,
Joe

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------





"This e-mail message is intended only for the use of the intended
recipient(s).
The information contained therein may be confidential or privileged, and
its disclosure or reproduction is strictly prohibited.
If you are not the intended recipient, please return it immediately to its
sender at the above address and destroy it."

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2