July 31, 2004
We had a military application wherein a tin plated box with electronics included therein had numerous tin whiskers growing therein. Since we had numerous fielded equipment we did not want to scrap, we repaired it by cleaning off the tin whiskers and then conformal coating with Type UR. Since that was done we had no further tin whisker problems. However, that does not necessarily mean that conformal coating prevents tin whisker growth. It could have been that once the tin whiskers were removed, the initial whisker growth removed the internal stress, and therefore, once the whiskers were cleaned off, no further whisker growth was noted, independent of whether or not we conformal coated the box.
----- Original Message -----
From: David Douthit<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Monday, July 26, 2004 10:46 AM
Subject: Re: [TN] Tin Whiskers
Edwin,
NASA did some experiments and have pictures on their web site
( http://nepp.nasa.gov/whisker/index.html<http://nepp.nasa.gov/whisker/index.html> ) of whiskers "punching"
through
coatings. I don't know if the coating "inhibited" growth (time, length,
or amount).
David A. Douthit
Manager
LoCan LLC
Edwin Louis wrote:
>Does anyone know whether a Polyurethane conformal coating would inhibit Tin
>whisker growth or at least contain it?
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-509-9700 ext.5315
>-----------------------------------------------------
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|