Here is further detail from the NPL database after registering to see defects. I don't know if Steve will want to contribute some of his defect pictures or not. Denny
From: [log in to unmask] [[log in to unmask]] on behalf of [log in to unmask] [[log in to unmask]]
Sent: Monday, March 16, 2015 4:14 PM
To: Fritz, Dennis D.; [log in to unmask]
Subject: NPL Assembly and Soldering Defect Database Online
Many thanks for registering on the National Physical Laboratory Defect Database. This is a live database and we will continue to add more defects to complement your online submissions: http://defectsdatabase.npl.co.uk
The database has over 100 defects that have been populated from cooperation with worldwide industry sources and from our own research studies. This has resulted in a unique resource, free for industry to use.
If you have a specific defect type not covered or have a current process problem with no solution please enter it on the database. http://defectsdatabase.npl.co.uk/forms/form3.html
If you have any other enquires or need technical assistance on a wide range of issues please contact Kate Clayton ([log in to unmask])
Many thanks,
Kate Clayton ([log in to unmask])
National Physical Laboratory
Hampton Rd | Teddington | Middlesex | UK | TW11 0LW
http://www.npl.co.uk
-----Original Message-----
From: Dennis Fritz <[log in to unmask]>
To: TechNet <[log in to unmask]>; pgoodyear <[log in to unmask]>
Sent: Mon, Mar 16, 2015 4:17 pm
Subject: Re: [TN] SMD failure pics
Pat.
The National Physics Lab in Great Britain maintains a photo galary of defects. It can be sorted by type of defect you want. Go to site
http://defectsdatabase.npl.co.uk/defectsdb/defects_query.php
You will have to enter a password and complete a simple security check to get in. Hope you can find what you need there.
Denny Fritz
-----Original Message-----
From: Patrick Goodyear <[log in to unmask]>
To: TechNet <[log in to unmask]>
Sent: Mon, Mar 16, 2015 1:54 pm
Subject: [TN] SMD failure pics
Hi All,
I'm helping some Ham Radio buddies out identifying failed SMD solder
joints. I have a ton of through hole pictures but alas no SMD
failures.
Does anyone have a few SMD typical failure pictures that I could
share.
They would be posted on the IC706MKIIg forum on Yahoo.com.
pat
goodyear ne6pg
Retired Control Technician
Pacific Gas and
Electric
______________________________________________________________________
This
email has been scanned by the Symantec Email Security.cloud service.
For more
information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|