Hi Mike! This is more of a question than a statement but would not
polyurethane particles char/burn/decompose if immersed in the wave
solderpot and end up being a constituent of the solderpot dross? I couldn't
find the char/flame resistance values for polyurethane but I am guessing
that they would not survive long in the solderpot (typical solderpot
temperature = 500F).

Dave Hillman
Rockwell Collins
[log in to unmask]




Michael Bell <[log in to unmask]>@ipc.org> on 07/18/2002 09:37:05 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
       to Michael Bell <[log in to unmask]>

Sent by:    TechNet <[log in to unmask]>


To:    [log in to unmask]
cc:

Subject:    [TN] Solder Pot Contamination


Hi all,

Has anyone ever come across a method in which to detect resin (polyurethane
particles) contamination in a Wave Solder Pot????  And in turn, a method to
remove this sort of contamination???

Cheers

Mike

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2