TECHNET Archives

June 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 23 Jun 2016 09:13:17 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
John Burke <[log in to unmask]>
Parts/Attachments:
text/plain (40 lines)
Good morning !!

 

A question came up on reliability testing.

 

Typically PCBA's are thermally cycled as a part of reliability testing
usually for 1000 cycles.

 

What is the group's experience for non-military thermal cycling ranges?.

 

I am often asked to use 0 - 100c sometimes -40 to 85c and sometimes various
other thermal cycles picked from the JEDEC standard.

 

What is the groups experience for this?. I am trying to establish "normal"
practice.

 

Best regards,

 

John



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2