HI Ivan! The purpose of the gold is to "protect" the Pd surface from
reacting with the environment. Pd is a "getter" material and can form a
number of "really neat" surface films, both oxide and/or organic films,
depending on the environment.
Dave Hillman
Rockwell Collins
[log in to unmask]
Ivanoe Pedruzzi
<i.pedruzzi@LABEL
GROUP.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
11/11/2005 04:36 Re: [TN] Gold plated components,
AM what a pain!!
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Ivanoe Pedruzzi
<i.pedruzzi@LABEL
GROUP.COM>
But Werner,
the 150 A is over Pd, does the Pd have different properties in terms
of oxidization, hence, soldering?
just for my understanding.
THX,
Ivan
Il giorno 10/nov/05, alle ore 23:16, Werner Engelmaier ha scritto:
> I agree that 150 Angstroms of Au "is pretty darn thin"--the problem
> is I see
> most layer thicknesses in the 500 to 1,000 A range. A 150A layer of
> au would
> not protect the Ni from oxidizing.
>
>
>
> Werner
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16 for additional information, or contact Keach Sasamori
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|