TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Fri, 10 Jul 1998 15:47:19 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (24 lines)
I am aware of the Dexter Dexcoat FST process. This is an organometallic tin
that places a barrier layer on the copper surface that greatly retards the
copper tin migration to a point that shelf life well in excess of one year is
easily achievable. This process produces a lead free planar surface that has
better solderability than Ni/AU. Some OEM's have claimed that this process is
the only alternative finish that they can run on the same assembly line with
HASL product and no changes need to be made. The key here is that the process
in not an ordinary immersion tin which would have a very limited shelf life.

Regards,
Chris McGary

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2