IPC-RB-276 has a chart defining minimum standard plating
thickness. for Gold the requirements are:

         Class 1    0.00075mm(0.00003in)
    general use PCBs
         Class 2    0.00075mm(0.00003in)
     high reliability PCBs
          Class 3   0.0013mm (0.00005in)
    mission critical PCBs
I hope this helps.

Jeffrey McGlaughlin
BFGoodrich Avionic Systems
Columbus Ohio


>>> starr devere <[log in to unmask]> 06/06/97 01:34pm
>>>
Is there an IPC spec for minimum thickness of gold plating
on edge tabs
for high reliability boards?  I was thinking it was 30
microinches but
I'm looking for a spec.
Thanks


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2