TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Phillip E. Hinton" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 29 Oct 1999 14:24:16 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (33 lines)
All

Per a previous request for information regarding the tensile and shear
strengths of solder alloys earlier this week :

Indium Corp has a web page which lists many of the properties of the solder
alloys.  It is www.indium.com.  The alloy physical property charts are a bit
hard to find so go to the left (ICA Navigator) of the starting web page and
click "products".  Then go to "Solder Fabrications" and click, go the
subheading "Alloy Physical Properties" and a page will come up that gives you
a selection of 4 pages to choose from.  The lower MP solder alloys are on the
first page while higher MP alloys are on the the last page.  Not all of the
blanks are filled in and not all of the alloys they furnish are listed,  but
they give you a number to call if you can not find the information.

The phone number is 1-315-853-4900 or 1-800-4INDIUM.

Phil Hinton

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2