TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Muhammad, Masdi" <[log in to unmask]>
Date:
Fri, 24 Jul 1998 10:09:08 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, superflx <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
superflx <[log in to unmask]>
Parts/Attachments:
text/plain (42 lines)
What is the type and viscosity of the flux you are using?

Phil

Muhammad, Masdi wrote:

>         We are trying to reduce the number of units fail at system test due
> to
> flux on gold finger.  We know so far that the flux is deposited onto the
> goldfinger during touch-up or rework and to reduce the contamination we are
> planning to implement 'taping' the gold finger during touch up.  Need some
> advice on what kind of tape we should use or is there any other simpler
> solution
> that we can implement.
>
> Appreciate the help.
>
> Masdi
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2