Hi Andy

The maximum elongation for eutectic solder to failure depends very strong
on the temperatrure and the strain-rate. If you deform solder very fast it
can not endure more than say 2%. If you induce a strain rate below 10 E-4
you can deform solder at room temperature over 100%. Heating the material
to 50°C will ease the problem to a considerable extend.

Guenter Grossmann