We have been starting to have solderability problems with some electroless
nickel plated pwbs.  Nickel has always been a challenge to solder... but we
have been successful until recently by simply doing a pumice scrub prior to
solder stenciling, and by minimizing the time through assembly and into reflow.

There have been a large number of Technet communications on Electroless Ni
and Immersion Au over the last few weeks.  We are tying to learn from those
who are having similar problems.

A few topics which were not fully addressed and would be of great value are:

1. Does anyone know of a good test coupon or test method which can be used
to evaluate pwb surface solderability?

2. What role does surface finish play in solderability and will a rough
plated Ni finish have more solderability problems than a smoother finish?


Any help would be appreciated.

Bill Dieffenbacher,  Lockheed Martin Control Systems
[log in to unmask]  Phone 607-770-2961  Fax 2056
_______________________________________________________________

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2