TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0uYvGX-0000GQC; Wed, 26 Jun 96 09:08 CDT
Content-Type:
text/plain; charset=us-ascii
CC:
References:
<960626094810.ZM13135@msaipc>
Date:
Wed, 26 Jun 1996 10:16:04 -0400
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/4860
TO:
Jesse F Beatty <[log in to unmask]>
Return-Path:
<TechNet-request>
X-Status:
X-Loop:
From [log in to unmask] Wed Jun 26 13:
37:53 1996
Content-Transfer-Encoding:
7bit
Resent-Message-ID:
<"jinjM3.0.hX8.IHKqn"@ipc>
Subject:
From:
[log in to unmask] (Doug McKean)
Old-Return-Path:
Message-ID:
Organization:
Paragon Networks Inc.
X-Mailer:
Mozilla 2.0 (Win95; I)
Parts/Attachments:
text/plain (51 lines)
Frank,

I have seen excellent conductivity measurements on bare concrete
floors at some houses that allows them to paint the floor with
industrial conductive paint.  It was cheaper for them to paint rather
than tile.  I have been at other houses where they had to tile because
the conductivity measurements of the concrete prevented painting causing 
them to "construct" a conductive floor with tile and grounding.

I have no information on the specific cost comparison between paint and 
tile for conductive flooring, but, do get a good set of 
reliable measurements on the conductivity of your floor before you 
begin.  You may need only paint.

Doug

Doug

Jesse F Beatty wrote:
> 
> --Hi Technet Gang...
> 
> This is not specifically a technical question, but I have run into a lack of
> information regarding this topic and decided to give the group a shot.
> 
> We are in the process of installing a new memory module assembly line and are
> looking at ways to improve the flooring in the area.  We are currently using
> static-resistant tiling which goes for roughly $8 a tile.  This particular
> flooring has some advantages, but we believe that there is a better, and perhaps
> less expensive, alternative.
> 
> Do any of you have experience with ESD flooring, either good or bad?  Can you
> suggest a particular type of flooring that we should consider or can you direct
> me to a source?
> 
> Please feel free to direct any replies to my personal address below.
> 
> Thanks, in advance, for your assistance.
> 
> 
> 
> THINK ABOUT IT:  Mediocrity is easy.  Good things take hard work.
> 
>                  Bob Seger (1995)
> 
> Frank Beatty                             Phone: 919/479-3552
> Memory Module Production Supervisor      Fax:   919/479-3546
> Mitsubishi Semiconductor America, Inc.   Email: [log in to unmask]



ATOM RSS1 RSS2