That may be the specified limit, but 1200 V/mm is one helluva gradient.
I certainly would not tolerate such a gradient for high-impedance
applications. I went as low as 25 V/mm when working at impedances of
>1E12 ohms with FR-4.
So, to plagiarise an outstanding contributor to this forum, I would say,
"it depends".
Brian
McGlaughlin, Jeffrey A wrote:
> Phil -
>
> IPC-2221 Table 6-1 covers electrical spacing column B1 applies to bare
> boards internal traces. The calculated spacing for 600V would be 0.5mm
> [0.020"].
>
>
> Jeffrey McGlaughlin, CID
> Engineering Designer
> Battelle
> 505 King Avenue
> Columbus Ohio 43201-2693
> (614)424-7582 Phone
> (614)458-7582 Fax
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
> Sent: Monday, October 15, 2007 10:29 AM
> To: [log in to unmask]
> Subject: [TN] inner layer spacing for voltage
>
> Good morning,
>
> One of our engineers posed this question;
>
> " I have an inner ground plane in an area with high voltage (to 600 V).
> My question is this: What is the recommended spacing between the
> plated-though hole with this voltage and the internal ground plane
> relief outline? I will go with 10 V/mil as a default, but I am hoping
> the safe limit might be a bit higher than this."
>
> Can you point me to an IPC spec for this? I was thinking it might be in
> 2222.
>
> Thanks in advance.
>
> Phil
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|