TECHNET Archives

July 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Chuck Brummer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 16 Jul 2015 07:49:56 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (163 lines)
Well then,  I stand behind my thinking these aren't pretty but my serve 
the intended purpose.

I agree that whoever made them needs to clean up their processing, the 
hole prep was poor.
The processing of the plate up image lacked too.

If you have a board to sacrifice I am sure many of us would like to see a 
X-section of the holes.

No electrical test cert?  Not to late to get them tested.

Chuck


Charles W. Brummer | 3M Manufacturing Engineer
3M Electronic Solutions Division
3M Canoga Park, 8357 Canoga Ave. | Canoga Park, CA 91304
Office: 818 734 4930
[log in to unmask] | www.3M.com


This message (including any attachments) may contain material, non-public 
information or proprietary information and is for the intended recipients 
only. If you are not the intended recipient, you should notify the sender 
and delete this message. Any disclosure, copying, or use of this 
information is strictly prohibited and may subject you to legal liability.



From:   "Ong Seet Leng" <[log in to unmask]>
To:     "TechNet E-Mail Forum" <[log in to unmask]>, "[log in to unmask]" 
<[log in to unmask]>
Date:   07/15/2015 04:56 PM
Subject:        [EXTERNAL] RE: [TN] MYSTRY DEFECT



No. It was just passed it to us for help in checking. No paperwork nothing 
to support.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chuck Brummer
Sent: Thursday, 16 July 2015 3:54 AM
To: [log in to unmask]
Subject: Re: [TN] MYSTRY DEFECT

or something that retards the copper plate up.
Not necessarily a problem, not pretty but not a problem if the hole walls 
are good.

If you section is the copper plate height requirement met?  If yes and 
they passed E test then they are good.

Did you get a micro section report with your certs?  Again, good micro 
section, good e test they are good, Hole walls have etch out, not so good.

that's my 2 cents,
Chuck


Charles W. Brummer | 3M Manufacturing Engineer 3M Electronic Solutions 
Division 3M Canoga Park, 8357 Canoga Ave. | Canoga Park, CA 91304
Office: 818 734 4930
[log in to unmask] | www.3M.com


This message (including any attachments) may contain material, non-public 
information or proprietary information and is for the intended recipients 
only. If you are not the intended recipient, you should notify the sender 
and delete this message. Any disclosure, copying, or use of this 
information is strictly prohibited and may subject you to legal liability.



From:   "Steve Gregory" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   07/15/2015 07:17 AM
Subject:        [EXTERNAL] Re: [TN] MYSTRY DEFECT
Sent by:        TechNet <[log in to unmask]>



Hi Ong Seet Leng,

I got your photos and have them posted now, the links are here:

http://stevezeva.homestead.com/Mystery_Defect_1.jpg

http://stevezeva.homestead.com/Mystery_Defect_2.jpg

Looks like there was some sort of problem with the etch resist, can't say 
exactly what that was though. I definitely would be kicking these back to 
the vendor!

Steve

On Tue, Jul 14, 2015 at 2:15 AM, Ong Seet Leng <[log in to unmask]>
wrote:

> Afternoon,
>
> I had checked a bare printed wiring board and attached a photograph on
one
> of the defect found. I would like to seek advice from you gurus' out
there
> on what to call this defect? For the life of me, I can't find the 
> definition of it. Appreciate if someone can guide me. Thanks in advance.
>
> Regards,
> Ong Seet Leng
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
[log in to unmask]
> ______________________________________________________________________
>

-- 


This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary 


or otherwise private information. Any unauthorized use, reproduction, 
dissemination, distribution or other disclosure of the contents of this 
e-mail or its attachments is strictly prohibited. If you have received 
this email in error, please notify the sender immediately and delete the 
original. 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________
3M security scanners have not detected any malicious content in this 
message.

To report this email as SPAM, please forward it to [log in to unmask]



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________
3M security scanners have not detected any malicious content in this 
message.

To report this email as SPAM, please forward it to [log in to unmask]



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2