TECHNET Archives

February 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Mon, 9 Feb 1998 08:22:19 PST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "John Haman Jr." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"; X-MAPIextension=".TXT"
From:
"John Haman Jr." <[log in to unmask]>
Parts/Attachments:
text/plain (34 lines)
Steve vs Gegory

        The number of insertions the gold fingers can withstand is directly
related to the thickness of the gold plate.   I've  manufactured boards in
the past
for computers with only 5- 8 millionths of gold required.  However,  I've
also manufactured
them with 30 - 50 millionths.  So depending on the manufacturing specs of
those boards
will tell you how long the gold will last.

        My recommendation is not to remove the boards every time a pm is done.
I would focus on keeping the equipment as clean as possible with scheduled
pm's
on a regular basis.  Every quarter or every six months I would clean the
finger contacts.
Watching for gold wear from the connectors.

John Haman Jr.
Process / Product Engineer
American Board Companies, Inc

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2