Silver tongues
Apr 17th 2008 | NEW YORK
From The Economist print edition
Regulators are looking more closely at nanotechnology claims
ANCIENT Phoenicians stored their drinking water in silver vessels, but not
for aesthetic reasons. They discovered that by doing so they remained
healthier. The reason for that is now understood: silver has antimicrobial properties.
In the 21st century people have realised that if you fortify Phoenician
wisdom with a dash of nanotechnology, silver can be made into a far more potent
bactericide. Companies have quickly seized on this idea to produce a wide
variety of products, from clothes to soap and even chopsticks, containing silver
nanoparticles. The claim is that they destroy germs.
But silver can also accumulate in the environment and, at certain levels,
prove toxic. Nor is the general safety of nanoparticles fully understood, not
least because they can react in novel ways. Some scientists think more research
is needed and perhaps more regulation too. A move in that direction now
seems to be under way.
Silver's natural germ-killing ability stems from its extremely slow release
of silver ions (electrically charged atoms, or groups of atoms). When made
into particles only a few nanometres big—a nanometre is a billionth of a metre—
they shed a lot more ions and so become more potent.
America's Environmental Protection Agency (EPA) is worried about a large
number of products claiming antimicrobial abilities. One is “Silver Wash”, a
washing machine made by Samsung, which claims to employ nanotechnology to
release hundreds of billions of silver ions during a wash to sanitise fabrics.
The EPA has ruled that ion-generating devices that claim to kill germs must
be registered as a pesticide and tested to show they pose no unreasonable
risk. The EPA says its intention is to regulate ion-generating devices rather
than nanotechnology itself. But it is hard to draw a distinction. Andrew
Maynard, chief science adviser for the Project on Emerging Nanotechnologies at the
Woodrow Wilson International Centre for Scholars in Washington, DC, says
functionality is an important part of the definition. Turning silver into tiny
particles that behave in new ways (for example, by shedding more ions) and
putting those particles into new places (such as fabrics) qualifies—or so he
thinks.
One consequence of dividing a substance into nanoparticles is that the
surface area of the material greatly expands. “Nanosilver is so tiny it can go
right to the surface of an organism and essentially shoot ions into the organism,
” says Sam Luoma, a research scientist at the John Muir Institute of the
Environment at the University of California, Davis. Although this makes silver
nanoparticles an extremely effective antimicrobial agent, it also raises
concerns about humans' ability to withstand relatively high exposures.
Despite the unknowns, Dr Luoma and others believe there is enormous potential
for good from nanosilver. It can, for example, be used in small amounts to
coat medical catheters to reduce the possibility of infection without causing
environmental worries. “We need to separate out the truly beneficial uses,”
he adds.
The EPA will not look at benefit or necessity, but is determined to make its
registration stick. It has fined one company more than $200,000 for making
unsubstantiated claims about unregistered nanosilver-coated computer mice and
keyboards. Firms making claims about nanotechnology need to watch out
**************Need a new ride? Check out the largest site for U.S. used car
listings at AOL Autos.
(http://autos.aol.com/used?NCID=aolcmp00300000002851)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|