Terry,
The question should be is why are you recieving boards with intermittent
opens from your board manufacturer.
It sounds like there is a serious design or manufacturing
flaw with this particular board. Are the opens in same location of the board
or are they random throughout the board?
Tony Steinke
AIT-Atlanta Inc.
----- Original Message -----
From: "Terry Exell" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, July 15, 2002 11:45 PM
Subject: [TN] Stress screening of multi layer production boards for optimum
reliability
> Dear All,
>
> I am experiencing occasional open circuits on 16 layer boards during
assembly and
> during in-service use. I have started thermal stressing all production
boards with
> the aim of screening out any boards with latent defects and this is
identifying and
> removing some problem boards. However, an equal number of problem boards
still
> fail during assembly.
>
> Does anyone use similar thermal stressing of production boards to help
improve
> assembly yields and product reliability? If so, do you find it
successful?
>
> My thermal stressing uses the following parameters:
> 10 cycles of hot / cold exposure in a HALT chamber,
> -60 deg C to +120 deg C temperature excursions,
> 40 deg C per minute temperature ramp rate.
> The boards are electrically tested after thermal stressing.
>
> I calculate the screening is using approximately 20% of the expected life
of the
> assembled boards, so I am reluctant to increase the stress levels.
>
> My board manufacturer has made several process improvements over the last
year but
> I have not seen a significant improvement in my assembly yield.
>
> Best regards
>
> Terry Exell
> PCB Assembly Engineer
> BAE SYSTEMS
> Plymouth, UK
>
>
>
> ********************************************************************
> This email and any attachments are confidential to the intended
> recipient and may also be privileged. If you are not the intended
> recipient please delete it from your system and notify the sender.
> You should not copy it or use it for any purpose nor disclose or
> distribute its contents to any other person.
> ********************************************************************
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|