TECHNET Archives

September 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 18 Sep 2003 04:48:58 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; charset=iso-8859-1
From:
Rudy Sedlak <[log in to unmask]>
Parts/Attachments:
text/plain (19 lines)
Are you etching with Cupric, or Ammoniacal etchant?  Ammoniacal is quite sensitive to tarnish on the board, so if your boards are tarnishing, this could be the problem...

What do the shorts look like?  Can you send us a picture?

Lots of resin spots popping up in the industry lately, not, of course, that I would want to blame the copper foil, or laminate from any particular part of the world... and this could be causing your problems...do you check laminat with black light as a part of inspection?  Might be a real good idea to begin, if you are not... One of the Sanmina's found innerlayer shorts almost completely related to resin spots on the Copper...

Good luck from Shenzhen China..
Rudy Sedlak, RD Chemical Company

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2