TECHNET Archives

July 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Guy Ramsey <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Date:
Mon, 4 Jul 2016 11:48:16 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (54 lines)
I was cleaning up a box of odds and ends that I kept from my old office
just last week and ran across a CD of Moon Man's book. He was an
interesting character, in imposing personality.

On Mon, Jul 4, 2016 at 11:39 AM, Inge Hernefjord <[log in to unmask]>
wrote:

> Hello, TN, Steve or Mike told me TN were going to rise a stone to honour
> me. In fact I am still alive even if I can only pulln'push 60 kilograms
> today and become drunk after only 10 centiliters of Jura. How's TN these
> days? Guess the total has lowered a bit and most fossils have left TN.  Not
> many today who knew Moon Man, hey.? Am impressed to hear Brian Ellis is
> still active.  Actually, we know fhat curmudgeons last much longer. Is
> Steven Creswick still acttive? Would like to have his email or URL.I have
> let go all techy stuff, doesn't interest me much any more, am with other
> words healed from brain artrocity caused by exaggerated sucking technical
> literature. I can dump a failing part without trying to repair it. And my
> many old soldering irons and stations have gone into the bin. So I am
> cured. I try to avoid images and photos from corroded boards or discussions
> about IMC. I forbid myself to pant over a screen showing porno, i.e. SEM
> images from BGAs and like. A photo on a high current density interface with
> areas of Gold migration could bring me back to former insane analysis
> addiction.. Ho-ho..nice to hear from ya'll. Semper fi/Inge
>
> On 23 June 2016 at 18:04, Graham Naisbitt <[log in to unmask]
> >
> wrote:
>
> > Hello fellow Techies,
> >
> > I thought you would all be pleased to know that my Global Operations
> > Manager, Nick Plumb and his wife, paid a visit to Brian and his wife
> > earlier this week whilst on vacation in Cyprus.
> >
> > They are both in fine fettle and Nick sent me a photo I will pass to
> Steve
> > to put on his web site - Steve?
> >
> > Brian was particularly happy to learn of the transition from ROSE to PICT
> > testing and of our recent success in achieving 6 Sigma Verification with
> > our equipment that he originally developed.
> >
> > Have a great weekend everyone,
> >
> > ATB - Graham Naisbitt
> >
> > ______________________________________________________________________
> > This email has been scanned by the Symantec Email Security.cloud service.
> > For more information please contact helpdesk at x2960 or
> [log in to unmask]
> > ______________________________________________________________________
> >
>

ATOM RSS1 RSS2