TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vMM86-0000R6C; Sat, 9 Nov 96 16:43 CST
Old-Return-Path:
Date:
Sat, 09 Nov 96 17:46:27 EST
Precedence:
list
Resent-From:
Cc:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/7564
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"MQkhQ1.0.CnM.jaGXo"@ipc>
Subject:
From:
From [log in to unmask] Thu Nov 14 10:
45:59 1996
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
Message-Id:
Parts/Attachments:
text/plain (25 lines)
We are currently looking into setting up a storage environment for our
prepregs.  I understand that if prepregs are kept up to 90 days that
they must be maintained at a temperature of less than 70 degrees F, and
between 30 to 50 percent humidity.  Can anyone tell me how they store
their prepregs, and maybe give me some names of companies that
manufacture refrigeration units specifically for this purpose.
is this still an open issue?  I may be able to provide some help.
          Please respond if prudent.
***************************************************************************
          * TechNet mail list is provided as a service by IPC using
          SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2