At 08:47 AM 9/9/96 EDT, you wrote:
>  I was wondering if someone has some information on the environmental impact
>of the parylene process.  Are there any emissions evolved and if so what are
>their typical concentrations?  I realize that some parylene may get trapped
>in the cold trap and will have to be disposed of by landfill.  How much waste
>is generated per cycle?
>  Also, I am told that substrates for parylene coating are first washed with
>de-ionized water and then treated with an adhesion enhancing solution.  In
>SCS's literature the enhancer is a gas while most companies use a liquid
>enhancer.  Are there any advantages/disadvantages with using either one?
>  Is humidity a problem for parylene?  Can humidty get trapped between the
>coating and the board which would cause corrosion?
>
>                   My thanks in advance.
>
>Reply:
>Per Ben Guthrie, an engineer in our area very familiar with Parylene:

Parylene is an excellent moisture barrier. Also, because it is applied using
a vacuum deposition process, 
moisture under the parylene is not likely. A pre-bake would take care of any
such concerns.
>
>
>
>
>
>
>
>
>
>
>
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To unsubscribe from this list at any time, send a message to:           *
>* [log in to unmask] with <subject: unsubscribe> and no text.        *
>***************************************************************************
>
>
>
----------------------------------
Jeffery L. Hempton              Phone: (219) 429-7335   Fax: (219) 429-4688
Hughes Defense Communications                           Mail Stop: 25-31
1010 Production Road, Fort Wayne, IN 46808-4106
Email: [log in to unmask]

"The reason most people do not recognize opportunity is because it is
usually wearing a pair of bib overalls and disquised as hard work."    -
-Thomas Edison

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2