Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Tue, 10 Sep 1996 09:59:08 -0500 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Resent-Message-ID: |
<"xmgyH3.0.LK7.p9ODo"@ipc> |
Subject: |
|
From: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0v0UIG-0000OuC; Tue, 10 Sep 96 10:00 CDT |
From [log in to unmask] Fri Sep 13 09: |
12:18 1996 |
X-Mailer: |
Windows Eudora Light Version 1.5.2 |
Message-Id: |
|
Parts/Attachments: |
|
|
At 08:47 AM 9/9/96 EDT, you wrote:
> I was wondering if someone has some information on the environmental impact
>of the parylene process. Are there any emissions evolved and if so what are
>their typical concentrations? I realize that some parylene may get trapped
>in the cold trap and will have to be disposed of by landfill. How much waste
>is generated per cycle?
> Also, I am told that substrates for parylene coating are first washed with
>de-ionized water and then treated with an adhesion enhancing solution. In
>SCS's literature the enhancer is a gas while most companies use a liquid
>enhancer. Are there any advantages/disadvantages with using either one?
> Is humidity a problem for parylene? Can humidty get trapped between the
>coating and the board which would cause corrosion?
>
> My thanks in advance.
>
>Reply:
>Per Ben Guthrie, an engineer in our area very familiar with Parylene:
Parylene is an excellent moisture barrier. Also, because it is applied using
a vacuum deposition process,
moisture under the parylene is not likely. A pre-bake would take care of any
such concerns.
>
>
>
>
>
>
>
>
>
>
>
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To unsubscribe from this list at any time, send a message to: *
>* [log in to unmask] with <subject: unsubscribe> and no text. *
>***************************************************************************
>
>
>
----------------------------------
Jeffery L. Hempton Phone: (219) 429-7335 Fax: (219) 429-4688
Hughes Defense Communications Mail Stop: 25-31
1010 Production Road, Fort Wayne, IN 46808-4106
Email: [log in to unmask]
"The reason most people do not recognize opportunity is because it is
usually wearing a pair of bib overalls and disquised as hard work." -
-Thomas Edison
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|