TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stephen R. Gregory" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 11 Oct 1999 18:58:28 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (38 lines)
Hi All!

Remember my little problem with dry-film mask flaking off after multiple
washes in Kyzen? Well, it's not that problem this time.

We went to a different vendor and they used a DuPont dry-film...passed all
the tests I through at it (thermal excursion through reflow, and multiple
cleanings) passed without so much as a scratch.

BUT I discovered another little problem now. We got our first batch of boards
and they matched the drawing which called out SMOBC. We got some boards
delivered a little later that were needed to complete the lot, and I noticed
a lighter color over the traces and vias than the boards we got sent to us
earlier. Me being a little "gun-shy" about masks, I looked at things a little
closer and removed some mask over one of the vias, and discovered that the
whole board had been gold plated. (there's PCI fingers on the board that need
the gold)

The big thing is that they didn't follow the drawing and give us SMOBC like
the drawing states, but is there any real performance problems that I should
be worried about? (Cripes! Can't things run smooth once inna while?)

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2