Hi All!
I'm just wondering if I'm missing something. Is there any performance reason
whatsoever, that requires solder mask over Tin/Lead instead of using SMOBC
(Solder Mask Over Bare Copper)?
Got a board in receiving inspection that I got called back to look at because
the mask was failing tape test. When I saw the board, it was solder mask over
Tin/Lead, just like it was called out on the drawing. The mask had already
lost adhesion in a few places, but we hadn't done anything to it yet
assembly-wise...
I see didn't see this particular boards drawing before we went out and bought
it, otherwise I would have thrown-up a red flag then. What suprised me
though, is that our fab vendor didn't say anything before they built it. Is anything
other than SMOBC being used regularly. I thought solder mask over Tin/Lead
was ancient stuff, and that everybody learned not to do that anymore...
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|