Hi Scott,
Your supplier is absolutely right. During reflow the MLB together with the
PTVs, RCs, CCs, SOT-23s reach the highest temperature during the reflow peak
(e.g. 221C) vs. a SOIC (216C) vs. 68 PLCC lead (205C) vs. 68PLCC body/die
(196C). From the last number you can see why the leads of components are slow
to heat; they are connected to quite substantial heat sinks.

Werner Engelmaier
Engelmaier Associates, Inc.
Electronic Packaging, Interconnection and Reliability Consulting
23 Gunther Street
Mendham, NJ  07945  USA
Phone & Fax: 201-543-2747
E-mail: [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2