As a good rule of thumb, if it does not affect the function or reliability of the intended use, then leave it alone. I only rework when absolutely necessary. I do not recommend reworking a part simply for the sake of meet spec. Specifications are guidelines generated by the end user to cover most issues. However, no specification can address every situation. If you are the end user and do not feel the nick will affect function or reliability, then use it as is. 

Sometimes we must apply common sense to our daily business decisions. 

Ed Cosper
Director Quality Assurance and Engineering 
Graphic Electronics Inc.
Tulsa, OK

----------
From:  gabriela[SMTP:[log in to unmask]]
Sent:  Tuesday, March 26, 1996 5:08 PM
To:  [log in to unmask]
Subject:  PCB   REPAIR

Hello,TechNetters!
Consider please the following problem:
Let's say,you have an expensive multilayer board with a nicked 
conductor.The nick narrows the conductor to 50%,but there is no 
problem concerning electrical performance.
Would you cosider repair with a welded covar strip?
Our supplier suggested the repair,but after seeing the mess around
it,I would much more prefer to use the board as it is.
Does anybody support this?

Thank you,
Gaby

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2