TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 19 Oct 2005 10:43:49 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin Asbell <[log in to unmask]>
Subject:
From:
Franklin Asbell <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (186 lines)
I agree with your opinion of conductive material fill. We try to teach our
customers the pros and cons of conductive fill when it is required on the
fab drawing or notes. We even have a few samples of how bad things can turn,
especially in the large plane area shown on that board.

What many people do not realize when coming up with what shall fill the via
is conductive materials...conduct heat...and when you have such a large area
as depicted...it's acting like a huge heat sink right in the critical area
of the board...

We recommend ceramic fill, there is no real change to the process, cost is
about the same...and the headaches are due to other reasons besides fill
material.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dwight Mattix
Sent: Wednesday, October 19, 2005 9:53 AM
To: [log in to unmask]
Subject: Re: [TN] Delamination at Thermal Via area?

We have a lot of experience w/ this type failure.  I'm working on the
assumption that there's a thermal via farm in that center gnd slug area.
A couple recommendations ff the cuff...
    * Stay away from conductive via fill material whenever possible when
vias are tightly packed in "thermal via farms."   Conductive fill is almost
never needed -- adds very little actual thermal/conductive benefit. We've
modeled it and test it.  For my money, conductive fill is almost always a
waste of time and a real pain in the patootie from reliability standpoint.
The biggest benefit is that it's easier to plate over and get good copper
adhesion and that usually only matters on probe sites. Esp
evil/unpredictable in this application is CB100 (I've had lots of dialogue
w/ Dupont over the years on this type failure).
    * Use a non-conductive fill that's more closely matched in CTE (e.g.San
eh) and don't overplate the fill.
    * Arguably the most significant factor:  don't plate over the thermal
vias.  All overplating does is give the fill something to push against and
force the whole plated area up during thermal excursions. It's like
screwing a cylinder head on tightly and then pushing all the pistons up
against it (expanding fill at temp).  Pop goes the weasel!  Overplating
doesn't add any grounding or thermal benefit. The solder joint in the gnd
slug will still be fine w/ the dot pattern that emerges.
    * As a work around/mod: We've eliminated a couple of these problems on
finished product by just etching or laser ablating a dot of copper off over
the fill.

there's my $.02.  Free and worth every penny.  ;^)

cheers,
dw

At 07:29 AM 10/19/2005, Steve Gregory wrote:
>Hi Wee Mei!
>
>I've got your pictures posted. Go to:
>
>http://www.stevezeva.homestead.com/files/U2_top.JPG
>http://www.stevezeva.homestead.com/files/U2_bottom.JPG
>http://www.stevezeva.homestead.com/files/U2_delamination.JPG
>
>Are the vias filled? Are you seeing this delamination on very many
>PCB's? Are you seeing it only on the bottom of the PCB?
>
>Kind regards,
>
>-Steve Gregory-
>Senior Process Engineer
>LaBarge Incorporated
>Tulsa, Oklahoma
>(918) 459-2285
>(918) 459-2350 FAX
>
>
>
>|---------+---------------------------->
>|         |           Wee Mei          |
>|         |           <[log in to unmask]
>|         |           SG>              |
>|         |           Sent by: TechNet |
>|         |           <[log in to unmask]>|
>|         |                            |
>|         |                            |
>|         |           10/19/2005 03:47 |
>|         |           AM               |
>|         |           Please respond to|
>|         |           TechNet E-Mail   |
>|         |           Forum            |
>|         |           <[log in to unmask]>|
>|         |           ; Please respond |
>|         |           to Wee Mei       |
>|         |           <[log in to unmask]
>|         |           SG>              |
>|         |                            |
>|---------+---------------------------->
>
>
>---------------------------------------------------------------------------
-----------------------------------|
>   |
>                                         |
>   |       To:       [log in to unmask]@SMTP@Exchange
>                                         |
>   |       cc:       (bcc: Stephen R
> Gregory/LABARGE)
|
>   |       Subject:  [TN] Delamination at Thermal Via
> area?                                                       |
>
>
>---------------------------------------------------------------------------
-----------------------------------|
>
>
>
>Hello,
>
>Just asked Steve to download 3 pictures on the defects. Kindly take a look
>at them and would appreciate some feedback on the possible root cause.
>
>Steve : Thanks for the downloading.
>
>Regards,
>Wee Mei
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>__________________________________________________________________
>This message may contain information that is privileged and confidential to
>LaBarge, Inc.  It is for use only by the individual or entity named above.
>If you are not the intended recipient, you may not copy, use or deliver
>this message to anyone.  In such event, you should destroy the message and
>kindly notify the sender by reply e-mail.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2