TECHNET Archives

March 2018

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Nutting, Phil" <[log in to unmask]>
Date:
Wed, 28 Mar 2018 19:15:11 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jose A Rios <[log in to unmask]>
Message-ID:
Subject:
From:
Jose A Rios <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Like Bhanu says, its design dependent, tough to pin down on an IPC document. In my previous role with a board fabricator, I was familiar with many bare board designs that would hold up to 40 or more ‘ambient to 230C' cycles with less than a 5% change in resistance, from ‘as received', on coupons representing the build (IPC-TM-650 2.6.26A, Method B), indicative those boards could holdup to more than just a handful of reflows. On legacy designs, you may be limited by material of construction and whether legacy methods of fabrication are to be preserved on those builds.





José (Joey) Ríos, Sr QA Engineer

Mission Assurance Manager

Kavli Institute for Astrophysics & Space Research

Massachusetts Institute of Technology

[log in to unmask]<mailto:[log in to unmask]>

(617)324-6272















On Mar 28, 2018, at 2:41 PM, Nutting, Phil <[log in to unmask]<mailto:[log in to unmask]>> wrote:



Our reworks are not to a single location, but rather various cuts, jumpers and component changes.  Some due to design issues of the existing board, change in operating points or obsolescence of the existing parts.



Only three reworks? Geesh, we surpassed that ages ago.



Having a magic number is easier for some folks to wrap their head around.  I'll pass along your suggestions.



Thanks,



Phil







-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman

Sent: Wednesday, March 28, 2018 2:07 PM

To: [log in to unmask]<mailto:[log in to unmask]>

Subject: Re: [TN] when is there too much rework on a circuit board



Hi team! I agree with Bhanu, having a fixed number requires established processes and material sets to be safe and even then, there is risk. Our current procedures allow for 3 reworks before a process/design team consultation/review is required.



Dave Hillman

Rockwell Collins

[log in to unmask]<mailto:[log in to unmask]>



On Wed, Mar 28, 2018 at 1:03 PM, Bhanu Sood <[log in to unmask]> wrote:



Rework or scrap? the risk is usually assessed by weighing in the

laminate type (PI, FR-4, flex etc), design, board stack-up, components

in vicinity of rework site and time/temperature required for each

rework (including preheat).





Any guidelines regarding the number of allowable reworks are going to

be specific to a design/material combination, tricky to extrapolate

that guidance into a standard…rework risk assessment needs to analyze

all factors and be better understood with solid research.  Most

companies say a site can be reworked 2 or 3 times (assuming high Td/Tg PI...$$$).







On Wed, Mar 28, 2018 at 1:40 PM, Nutting, Phil

<[log in to unmask]



wrote:



Respected colleagues,



I was just asked a question to which I could not put a number.



In the case of needing to fix a circuit board "right now" to fill

the income stream there should be a logical point at which the

reworks have become too extensive for production boards beyond the

"right now" need

and

the board should be revised to eliminate the reworks.



Is there an IPC or MIL standard that suggests a limit on the number

of or amount of rework allowed on a circuit board before it should be revised?





Phil Nutting  |  HVP Senior Development Engineer   |  Excelitas

Technologies Corp



Lab: +1 978.224.4332   |  Office: +1 978.224.4152

35 Congress St, Salem, MA  01970 USA

[log in to unmask]<mailto:[log in to unmask]>

www.excelitas.com<http://www.excelitas.com/>





[Excelitas R_emailsig]





Please consider the environment before printing this e-mail.

________________________________

This email message and any attachments are confidential and

proprietary

to

Excelitas Technologies Corp. If you are not the intended recipient

of

this

message, please inform the sender by replying to this email or

sending a message to the sender and destroy the message and any

attachments. Thank you.









--

Bhanu Sood

Tel: (202) 468-8449






ATOM RSS1 RSS2