text/plain (32 lines)
We are just starting to manufacture a PCB with a .039" fine-line PBGA.
We are currently seeing voids, mainly in the center, that are as much
as 45%. We also intermittently see the corner balls of the PBGA
smaller than the center balls. We are using a 6-mil stencil with a 1:1
aperture size (.019" mil). We are using a convection oven and
reflowing in air. The solder paste is an OA 62SN36PB02AG and the
reflow profile is:
Preheat - 0-150 degrees C in 90 sec
Soak - 150-189 degrees C for 120 sec
Reflow - 189-210 degrees C for 60 sec
Thermocouples were attached to both the corner and center of the PBGA
and they both had the exact same profile with a max temp of 210
Degrees C.

Does anyone have any recommendations for minimizing the amount of
voiding? Is 45% voiding acceptable? What would explain the corner
balls being smaller than the center balls?

Thank you for your input.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2