TECHNET Archives

December 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Poh Kong Hui <[log in to unmask]>
Date:
Thu, 10 Dec 1998 23:20:25 +0800
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Poh Kong Hui <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Hi Technetters,

Pardon my innocence. I am very curious to find out whether there is
taping or masking need to be done on the goldfinger before applying
the OCC material.

I understand that OCC can act as an insulator. So if there is no
masking on goldfinger, will the heat from the reflow oven able to
completely burn off the OCC material ?

Could you pls advise me.


Poh

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2