Mr. Hillel,

The gold thickness does affect connector reliability. Following factors
are critical and affect choice of gold thickness:

1. Contact force
2. Type of gold, soft or hard
3. Substrate roughness
4. Number of insertions required
5. Connector design, Zero insertion force vs. normal insertion
6. Environmental conditions during use (Corrosion)
7. Gold plating porosity
8. Base Nickel plating porosity

Based on reliability, 30 microinch seems a good choice.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2